A182-F11, A182-F12, lan A182-F22 kabeh kalebu kelas baja paduan sing umum digunakake kanggo macem-macem aplikasi industri, utamane ing lingkungan suhu dhuwur lan tekanan dhuwur. Kelas kasebut nduweni komposisi kimia lan sifat mekanik sing beda-beda, saengga cocog kanggo macem-macem jinis aplikasi. Baja iki utamane digunakake ing sistem tekanan, kalebu flensa, fitting, katup lan bagean sing padha, lan digunakake sacara wiyar ing pabrik petrokimia, konversi batu bara, tenaga nuklir, silinder turbin uap, tenaga termal lan peralatan skala gedhe liyane kanthi kondisi operasi sing atos lan media korosif sing kompleks.
KOMPOSISI KIMIA BAJA F11TION
| Tingkat | Kelas | C | Si | Mn | P | S | Cr | Mo |
| Kelas 1 | F11 | 0.05-0.15 | 0.5-1.0 | 0.3-0.6 | ≤0.03 | ≤0.03 | 1.0-1.5 | 0.44-0.65 |
| Kelas 2 | F11 | 0.1-0.2 | 0.5-1.0 | 0.3-0.6 | ≤0,04 | ≤0,04 | 1.0-1.5 | 0.44-0.65 |
| Kelas 3 | F11 | 0.1-0.2 | 0.5-1.0 | 0.3-0.6 | ≤0,04 | ≤0,04 | 1.0-1.5 | 0.44-0.65 |
KOMPOSISI KIMIA BAJA F12TION
| Tingkat | Kelas | C | Si | Mn | P | S | Cr | Mo |
| Kelas 1 | F12 | 0.05-0.15 | ≤0.5 | 0.3-0.6 | ≤0.045 | ≤0.045 | 0.8-1.25 | 0.44-0.65 |
| Kelas 2 | F12 | 0.1-0.2 | 0.1-0.6 | 0.3-0.8 | ≤0,04 | ≤0,04 | 0.8-1.25 | 0.44-0.65 |
KOMPOSISI KIMIA BAJA F22TION
| Tingkat | Kelas | C | Si | Mn | P | S | Cr | Mo |
| Kelas 1 | F22 | 0.05-0.15 | ≤0.5 | 0.3-0.6 | ≤0,04 | ≤0,04 | 2.0-2.5 | 0.87-1.13 |
| Kelas 3 | F22 | 0.05-0.15 | ≤0.5 | 0.3-0.6 | ≤0,04 | ≤0,04 | 2.0-2.5 | 0.87-1.13 |
PROPERTI MEKANIK BAJA F11/F12/F22
| Kelas | Tingkat | Kekuwatan Tarik, Mpa | Kekuatan Asil, Mpa | Pemanjangan,% | Pangurangan Jembar,% | Kekerasan, HBW |
| F11 | Kelas 1 | ≥415 | ≥205 | ≥20 | ≥45 | 121-174 |
| Kelas 2 | ≥485 | ≥275 | ≥20 | ≥30 | 143-207 | |
| Kelas 3 | ≥515 | ≥310 | ≥20 | ≥30 | 156-207 | |
| F12 | Kelas 1 | ≥415 | ≥220 | ≥20 | ≥45 | 121-174 |
| Kelas 2 | ≥485 | ≥275 | ≥20 | ≥30 | 143-207 | |
| F22 | Kelas 1 | ≥415 | ≥205 | ≥20 | ≥35 | ≤170 |
| Kelas 3 | ≥515 | ≥310 | ≥20 | ≥30 | 156-207 |
Bentenane utama antarane baja paduan A182-F11, A182-F12, lan A182-F22 ana ing komposisi kimia lan sifat mekanik sing diasilake. A182-F11 nawakake kinerja sing apik ing suhu sedheng, dene A182-F12 lan A182-F22 nyedhiyakake kekuatan lan resistensi sing luwih dhuwur marang korosi lan creep suhu dhuwur, kanthi A182-F22 umume dadi sing paling kuat lan paling tahan korosi ing antarane telu kasebut.